Re: [MW:15798] E8018-B8 instead off E8015-B8

Check about impact requirements because of AWS clasification. QW404.12.

Regards,
Valeria




De:        sudalai kannan <sudalaims@gmail.com>
Para:        materials-welding@googlegroups.com
Fecha:        28/10/2012 22:23
Asunto:        [MW:15789] E8018-B8 instead off E8015-B8
Enviado por:        materials-welding@googlegroups.com




Dear Experts,

Can i use E8018-B8  instead off E8015-B8, My PQR ware done with E8015-B8, 

If i need to use 8018-B8, what is the restructions ?


Please give me the solution/.

with regards,
M.Sudalai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

__________________________________________________________________  La información contenida en este mensaje es confidencial, y puede ser usada exclusivamente  por aquellas personas a las cuales está dirigida, dentro de los límites establecidos para   su uso. Si este mail es recibido por error, agradeceremos a su receptor tenga a bien informar   esa circunstancia al emisor, dirigiendo el mensaje a la dirección de correo electrónico que  lo haya remitido. En tal hipótesis, además, se solicita no copie ni revele el mensaje, como   así tampoco divulgue su contenido a terceras partes, para evitar un eventual comportamiento   ilícito. Las opiniones contenidas en este mensaje son exclusivas de su emisor y no representan   necesariamente la opinión de la empresa.    The information contained in this message is confidential, and is intended exclusively for the   individuals who have been specifically addressed, considering the limitations established for   its use. If this mail is received by error, please inform the sender and return the message   to the email address that had sent it. In such case, please do not copy or disclose the   message or its contents to any third party in order to avoid any unlawful conduct. The statements   included in this message belong only to the sender and do not necessarily constitute the   company s view.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...