Re: [MW:15795] E8018-B8 instead off E8015-B8


IMO, both are low hydrogen electrodes and fall under same F number and hence you can proceed.

Respectfully,

Nandesh Kumar A


--- On Sun, 28/10/12, sudalai kannan <sudalaims@gmail.com> wrote:

From: sudalai kannan <sudalaims@gmail.com>
Subject: [MW:15789] E8018-B8 instead off E8015-B8
To: materials-welding@googlegroups.com
Date: Sunday, 28 October, 2012, 12:44 PM

Dear Experts,

Can i use E8018-B8  instead off E8015-B8, My PQR ware done with E8015-B8, 

If i need to use 8018-B8, what is the restructions ?


Please give me the solution/.

with regards,
M.Sudalai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...