Re: [MW:15783] Why do we Use of clamps instead of TackWelds in pipeline?

Dear ,
 
It is for the ease of construction for continious pipe line to do fast welding .Tacking and weld removal is a time taking job for the completion of welding
 
Regards
Rajesh

--- On Fri, 10/26/12, srinivas rao <ksrvasu@gmail.com> wrote:

From: srinivas rao <ksrvasu@gmail.com>
Subject: [MW:15775] Why do we Use of clamps instead of TackWelds in pipeline?
To: materials-welding@googlegroups.com
Date: Friday, October 26, 2012, 1:01 AM

Dear Gents,

Can anyone clarify Why can't we use tack weld for fit-up in pipeline?

Regards

Srinivas
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...