Dear Srinivas,
 
It's depend on field temperatures and long line-pipe section stress,that's why we never recommend tack weld in pipeline
always used external & internal clamp for joint fit up.Tacking method possible only in station piping.
On Fri, Oct 26, 2012 at 11:31 AM, srinivas rao <ksrvasu@gmail.com> wrote:
Dear Gents,

Can anyone clarify Why can't we use tack weld for fit-up in pipeline?

Regards

Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Thanks & Regards,

Amit,
Inspection Engineer,
ABSIV,Bhogat Terminal,
Jamnagar,Gujarat.
Cell No. :- +91-9891069626 (Delhi)
                +91-8141323401 (Gujarat)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...