It is allowed as per section viii div 1 uh 37(h)

Vijay malusare

On Oct 25, 2012 4:53 PM, "Amit Udavant" <amitudavant@gmail.com> wrote

>
> Dear Experts
> We are a fabrication company  fabricating the Staic Equipments.
> This query is regarding the RF Pad for the manhole in a vessels Dished End.
> The Dished End is 14 thk ,MOC IS2062 Having a manhole RF Pad of 900 OD and 620 ID  X 14thk.
> Does the ASME Sec VIII DIV 1 allow  attachment of the RF pad for a nozzle/manhole in more than 1 Part.ie does the code permit the attachment of RF pand in two half as it is joined by the fillet welds.
>
> --
> Warm Regards
> amit 9833859030.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>  
>  

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...