Friday, October 26, 2012

Re: [MW:15772] Requirement of PWHT in categorie D

Hi!
My interpretation is as Weld metal th is more than 38mm (Base meta +RF pad) which is continuous thk Therefore It require PWHT
( However some of the Designer  do not consider RF pad weld thk in calulating effective thk in such case you may not require PWHT)
My interpretation is PWHT is required for your case

Regards

Hegde P.B.

--- On Fri, 26/10/12, g.venkatesan06@gmail.com <g.venkatesan06@gmail.com> wrote:

From: g.venkatesan06@gmail.com <g.venkatesan06@gmail.com>
Subject: [MW:15768] Requirement of PWHT in categorie D
To: materials-welding@googlegroups.com
Date: Friday, 26 October, 2012, 8:54 AM

Dear sir.
Kindly replay the below mail
regards
venkat

----------
Sent from my Nokia phone

------Original message------
From: g.venkatesan06@gmail.com <g.venkatesan06@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, October 25, 2012 2:56:08 PM GMT+0000
Subject: Requirement of PWHT in categorie D

Dear experts,
we are doing welding in a vessel of joint nozzle to dish with reinforcement pad(pipe thick 10mm(32inch), dish thik 20mm & RF pad 20mm) the weld detail in drawing shows bevel(55 degree) followed with fillet(10mm). All are P1 material.
In my question : the total weld metal deposit is 50mm in a joint(40mm CJP & 10 Fillet)
code says above 38mm groove weld for P1 material PWHT is mandatory and also says groove & fillet exceed 26mm in 2inch pipe PWHT is required.
Now we will do PWHT or not in a particular joint. If not kindly tell the reason.
Regards
venkat
welding engineer
trichy.

----------
Sent from my Nokia phone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...