Re: [MW:15760] RE: 15748] Regarding p91 intermediate cooling

That's right Pradip, lets always keep basic metallurgy in mind

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

"pgoswami" <pgoswami@quickclic.net>


    "pgoswami" <pgoswami@quickclic.net> 
    Sent by: materials-welding@googlegroups.com

    25/10/2012 02:25

    Please respond to
    materials-welding@googlegroups.com

To

    <materials-welding@googlegroups.com>

cc


Subject

    [MW:15758] RE: 15748] Regarding p91 intermediate cooling

Ref


Hi Govindaraju,
 
This temperature corresponds to the Martensite finish temperature for this steel.Grade-91 is thorough hardening steel and produces martesite on air cooling. The best room temperature mechanical properties (tensile, impact and hardness) for this steel  and the best high temperature creep properties are achieved when this steel is in fully tempered martensitic condition, i.e tempered @ 740-780 Deg C, following welding
 
Cooling to this temperature ,80c-110C  immediately following welding  but prior to PWHT is strongly advisable.
 
Thanks.
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of GOVINDARAJU RAJU
Sent:
 Tuesday, October 23, 2012 4:43 AM
To:
 materials-welding@googlegroups.com
Subject:
 [MW:15748] Reagrdin p91 intermediate cooling

Dear sir
 I am doing qc engineer in power plant construction.I have doubt regarding P91 welding.After completion of welding, we are doing intermediate cooling at 80c-110C.What is the  need of intemediate cooling?
 
Rgds
V.GOVINDARAJU
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
NOTICE: This message contains information which is confidential and the copyright of our company or a third party. If you are not the intended recipient of this message please delete it and destroy all copies. If you
are the intended recipient of this message you should not disclose or distribute this message to third parties without the consent of our company. Our company does not represent, warrant and/or guarantee that the integrity of this message has been maintained nor that the communication is free of virus, interception or interference. The liability of our company is limited by our General Conditions of Services.
Nota : Ce message contient des informations confidentielles propriété de notre société et/ou d'un tiers. Si vous n'êtes pas parmi les destinataires désignés de ce message, merci de l'effacer ainsi que toutes ses copies. Si vous êtes parmi les destinataires désignés de ce message, prière de ne pas le divulguer ni de le transmettre à des tiers sans l'accord de notre société. Notre société ne peut garantir que l'intégrité de ce message a été préservée ni que la présente communication est sans virus, interception ou interférence. La responsabilité de notre société est limitée par nos Conditions Générales de Services.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...