Dear Chandrakant,
Clause 323.4 -b clearly states that if the thickness reduce below 80%
then only you have to go for reduction in temp. In your case it is not
require to reduce the temperature as you are not reducing the
thickness below 80%
And for the average value you have to refer the table 323.5 and
consider the minimum tensile strength of the either material.i.e if SA
333 gr6 have min. tensile strength value 60 and Sa350 have min.
tensile strength value 70 then you have to consider the value 60 from
table.
Hope that this information is helpfull to you.
Best Regards,
Vikas P. Waghmare
Bureau veritas
Abudhabi
On 10/20/12, chandrakant yadav <yadav.chandrakant@gmail.com> wrote:
> Dear experts
> I have a dout in the interpretation of the sub
> size,impact value and the temprature reduction as per asme 31.3 table
> 323.3.4) and the material code (asme sec 12A for sa350 LF2,333GR6
> table 5 and table 6 )
> question is :- If the test piece is 3 inch sch 40 (thicknes 5.49)
> and the thickness of the machined specimen for the impact is 5 mm
> (more than the 80% thickness of the test specimen).do we have to
> perform the impact test on the specimen what will be the test
> temprature -46 deg centigrade or -57 deg centigrade.
> and what will be the impact value required for single and average.
>
>
>
>
> --
> With Kind Regards,
>
> Chandrakant Yadav
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment