Dear experts,

1.while performing a Hydro static test in a pipe line/spool at two different elevation for a continuous one line ,one pressure gauge  has found one reading  at one elevation and another pressure gauge has found another reading at another elevation how much can be the pressure variation in the Two pressure gauges as temperature is also a factor how much temp variation can be allowed as per code???

2.How much percentage of  increase in testing pressure can be increased in testing a pipe line for HST for a specific Testing pressure given in the Drawings???  

3.Please clarify whether Socket weld is Circumferential welding or not define types of circumferential joints???


DASARI SRIKANTH

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...