Hi All,
   Pls find below table of Valve parts and material data, Pls help me to get the right material  and appreciate, if you can describe the difference of thes 2 materials.
 
Details.
Valve - 7500 PSI BW Gate.
Fluid - Water / oil based mud.
Design Press - 7500 PSI.
Design Temp - 150 F.
 
Description.
 
                                    Option 1.                                                Option 2.
 
1, Body                     - ASTM A487 Gr 4 Class D.                     ZG30CrMo(4130)Casting.
2, Gate                     - 17-4 PH SS.                                            4130 + Nitriding.
3, Body wear ring     - AISI 4140 w/QPQ nitride coating.           4130.
4, Seat and Stem     - 410 SS.                                                   4130 + Nitriding.
5, Housing                - AISI C 1029.                                           4130.
 
 
How can I have more knowledge in material selection, especially valves. Pls provide me the info of Stes or Links.
Many Thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS