Tuesday, October 23, 2012

[MW:15748] Reagrdin p91 intermediate cooling

Dear sir
 I am doing qc engineer in power plant construction.I have doubt regarding P91 welding.After completion of welding, we are doing intermediate cooling at 80c-110C.What is the  need of intemediate cooling?
 
Rgds
V.GOVINDARAJU
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 