Thursday, September 13, 2012

Re: [MW:15289] Impact Test clarification

Dear Expert Team,
Query:-
In the same example as per trail mail,

If the test coupon have failed in impact testing only & rest of tests (Tensile,Bend,hardness etc) have passed in a PQR (So WPS is qualified without impact test requirement),BY Welder A
 
 then is it required to redo all the Welding proocedure (along with impact test & to be carried out in next PQR to support the previously qualified WPS.
"Can We performed or Carry out welding with BY WELDER B "

regards,
Ashish
On Wed, Sep 12, 2012 at 9:19 AM, Ashish Pathrabe <darkash6633@gmail.com> wrote:
Dear hiren,

"only impact test to be carried out in next PQR to support the previously qualified WPS".
Ashish P


On Tue, Sep 11, 2012 at 12:25 PM, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Experts,

In the same example as per trail mail,

If the test coupon have failed in impact testing only & rest of tests (Tensile,Bend,hardness etc) have passed in a PQR (So WPS is qualified without impact test requirement), then is it required to redo all the mechanical testing (Tensile,Bend,hardness etc) along with impact test or only impact test to be carried out in next PQR to support the previously qualified WPS.

Thanks & Regards

Hiren Sevak

On Mon, Sep 3, 2012 at 8:03 AM, mubeen mubeen <mubeenaws@gmail.com> wrote:
Dear experts, 

Please help out to clear my doubt. 

I have qualified a WPS/PQR with impact -29 deg C, now customer want the WPS/PQR shall be qualified with impact in -46 deg C. Also there is no remaining coupon piece available for impact testing with -46 deg C. 

My question here is, should I weld a coupon and only do impact test as required by customer and attached to PQR will be sort out this issue.? 
or 
Should I REDO a PQR with all mechanical  test which includes Tensile, Hardness, Bend along with impact will sort our this issue.? 


Requesting you to please provide me ASME IX clause reference.


Anticipating for you kind help. 

Thanks & Regards. 
M.K.Mubeen

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...