dear sutar,

there is no maximum dia limit for spin holes in dished ends as per code. generally it ranges from 25 mm to 40 mm.
if there is no nozzle at that location than patch shall be welded and 100% radiographed which is code requirement.

Regards
Sanjay Yadav

On Thu, Sep 6, 2012 at 9:16 AM, hemant <hsuthar@chemithon.co.in> wrote:

Dear Sir,

What is the minimum  & Maximum size of spin hole plate as per code reference. Pls reply me.

 

HEMANT SUTHAR

QA/QC

CEPL-SILVASSA

9712973092

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...