RE: [MW:15215] Impact Test clarification

Dear Sudhakar,

 

Apologies if my understanding is wrong, Sec 9 says that variation in supplementary essential variables require requalification of WPS ref:200.1.C.

 

Hope you will update.

 

Thanks and regards,

 

Arun S Das

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sudhakar kuppuswamy
Sent: Monday, September 03, 2012 11:49 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:15197] Impact Test clarification

 

 

Dear Mubeen,

 

No need to REDO the entire test.

 

You can weld a test coupon by using the existing WPS and only Impact test shall be carried out at -46 deg C.

 

 

Heat input shall be controlled during test coupon welding and H.I values shall not exceeds the previous qualified PQR value and ensure other essential shall be as per previous qualified PQR.

 

As per ASME SEC 09 clauses /tables from QW 252 through QW 266, increase in heat input is a supplementary essential variable. This refers to QW 409.1.

 

please refer to the above mentioned  clause in  ASME SEC 09.

 

 

Regards,

Sudhakar.K

 

 

 

 

On Mon, Sep 3, 2012 at 6:33 AM, mubeen mubeen <mubeenaws@gmail.com> wrote:

Dear experts, 

Please help out to clear my doubt. 

I have qualified a WPS/PQR with impact -29 deg C, now customer want the WPS/PQR shall be qualified with impact in -46 deg C. Also there is no remaining coupon piece available for impact testing with -46 deg C. 

My question here is, should I weld a coupon and only do impact test as required by customer and attached to PQR will be sort out this issue.? 
or 
Should I REDO a PQR with all mechanical  test which includes Tensile, Hardness, Bend along with impact will sort our this issue.? 

 

 

Requesting you to please provide me ASME IX clause reference.

 


Anticipating for you kind help. 

Thanks & Regards. 
M.K.Mubeen

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


 
Nota di riservatezza : Il presente messaggio, corredato dei relativi allegati, contiene informazioni da considerarsi strettamente riservate, ed è destinato esclusivamente al destinatario sopra indicato, il quale è l'unico autorizzato ad usarlo, copiarlo e, sotto la propria responsabilità, diffonderlo. Chiunque ricevesse questo messaggio per errore o comunque lo leggesse senza esserne legittimato è avvertito che trattenerlo, copiarlo, divulgarlo, distribuirlo a persone diverse dal destinatario è severamente proibito, ed è pregato di rinviarlo immediatamente al mittente distruggendone l'originale.
Grazie

Confidentiality Notice : This message, together with its attachments, contains strictly confidential information and is intended only for the addressee identified above, who is the sole party authorized to use and copy it and, assuming any related liability , to forward it to others. Anyone receiving this message by mistake or reading it without authorization is hereby notified that storage, reproduction, disclosure or distribution of the message to persons other than the addressee is strictly forbidden. They are asked to return the message immediately to the sender and to erase the original message received.
Thank you

 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...