Dear Expert,

For Vessel (ASME Sec. VIII Div. 1), 
Shell Material = SA 516 Gr. 70N (P. 1 G. 2) Impact Test required per code
Nozzle Pipe Material = SA 333 Gr. 6 (P. 1 G. 1) Impact Test is not Required per code

Can we use a WPS qualified with P.1 G.2 only to weld Nozzle to Shell joint in above mentioned Vessel.

Thanks


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...