Monday, September 10, 2012

[MW:15260] Use of ASME IX WPS for Dissimilar Thickness of More than Range of Groove Weld Thickness Qualified?

Dear All,

Please advise whether A WPS qualified per ASME Sec IX. with PQR Thickness 20mm, can be used for below Joint as shown below, with dissimilar thickness of 92mm and 30mm? As shown in below figure.
Kindly Give Sec, IX clasue reference if possible.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...