[MW:15244] Hard facing on Hammer IS;276 Mn steel Gr.III Reg.

Dear Experts,

 

         As per Client Requirement Hard facing is Required  on the Hammer Mn steel Gr.III and Hardness should be maintain 400 to 500BHN.10mm thk Hardfacing is required on four side

    Now are doing Hardfacing on the Hammer. First we are making Buffer layer with FCAW process and than we are used GMAT-3200 Electrode  for Hard facing.

 

  But problem is that after welding Hard Facing are found crack at so many place.


   So kindly Give us your Valuable feedback to resolve our matter.

 


--
Regards,

Bhupendrasinh Gohil
MSEL
BARODA
GUJARAT
(Mob.)09687322281
Araise and awake untill u reach the goal.....                          
       

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...