Dear 
The velocity of air inlet is more than inside of the box. So it evacuate the air inside the box and create vacuum. We are not passing the air directly inside, air passed through the straight pipe and a branch only connected with it. The simple mechanism like our bed buck sprayer pump (mini).

 

On 12 May 2012 08:22, M S <striarc@gmail.com> wrote:
Friends,

Enlighten me that How vacuum is created by feeding air by air compressor inside the vacuum box during test?(reference materials for vacuum test shows air is feeding into to the vacuum box)

Regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...