Re: [MW:14244] Any where mentioned about welding machine calibration is required for pipeline

Hi,
You have not mentioned, which code you are following
for your production/fabrication weld.
In API 6A para 6.3.2.7 -  welding controls specify as below:
" Instruments to indicate temperature,voltage,and ampearage shall be serviced and calibrated in accordance with the manufacturers written specification"
 
Manivannan.

 
On Fri, May 11, 2012 at 8:14 AM, mpk mpk <ranmi2007@gmail.com> wrote:
Dear Experts,

Any where mentioned about welding machine calibration is required for pipeline.need Reference.

Thank you,
Yem Pee.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
MANIVANNAN.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...