Yes in pipe line welding for cs to ss welding to achieve good penetration it is required.
Thanks & Regards, Mukesh Chaudhari Oriental Manufacturers Private Limited Ranoli -391 350 Baroda Gujarat India T: +91.265.223 1663/2232936 F: +91.265.223 0171 |
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vinod Kataria
Sent: 15 May 2012 17:06
To: materials-welding@googlegroups.com
Subject: [MW:14265] RE: 14262] For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required
Yes it is required.
With kind regards,
Vinod Kumar Kataria
GM - Operations
Bliss Anand Private Limited,
92B/93B Sector 5
IMT Manesar,Gurgaon,
National Capital Region Delhi.
India .
Phone : +91-124-4366000 (9 Lines)
Mobile Phone : +91-9560199004
Fax : +91-124-2290884
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mpk mpk
Sent: Tuesday, May 15, 2012 8:39 AM
To: materials-welding
Subject: [MW:14262] For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required
Dear Experts,
For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required ?
Thank you
Yem Pee
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment