[MW:14231] RE: 14217] Flux-Electrode Combination required.

Dear Ansari

 

Further to the comments given by other experts, you can try with EM12K / EH14 & Suitable Flux. But as the thickness is 70mm, you can try using Basic flux ( Non-Active Flux) to avoid C , Mn pick up , specially when you do multi pass SAW welding. In some cases, we have observed high hardness (260-280BHN) due to this pick up.

 

You can try with F7P2EM12K, F7P4EH14, F7P2EH10K etc.

 

Regards

Fredric Prabu. K

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ansari intekhab alam
Sent: Tuesday, May 08, 2012 3:55 PM
To: materials-welding@googlegroups.com
Subject: [MW:14217] Flux-Electrode Combination required.

 

Dear Experts 

Hi ,

further can anyone suggest me that the electrode for SMAW  and Electrode and flux wire combination for SAW Process.

Details as are

1. Material - SA 516-70

2.Thickness-70 mm

3.Normalizing-  ( 920 Deg - 150 min )  +  Dress relieving ( 620 Deg - 350 Minutes ).

also please suggest that how we can choose the electrodes and fluxes for a particular weld by using ASME Section 2 Part C.

 
-
Regards
Ansari Intekhab Alam

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...