Mr. Ansari,
  • What's the design code?
  • any impact test requirements
  • any hardness requirements?
 
Appreciate your response.
 
Thanks.
 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ansari intekhab alam
Sent: Tuesday, May 08, 2012 6:25 AM
To: materials-welding@googlegroups.com
Subject: [MW:14217] Flux-Electrode Combination required.

Dear Experts 
Hi ,
further can anyone suggest me that the electrode for SMAW  and Electrode and flux wire combination for SAW Process.
Details as are
1. Material - SA 516-70
2.Thickness-70 mm
3.Normalizing-  ( 920 Deg - 150 min )  +  Dress relieving ( 620 Deg - 350 Minutes ).
also please suggest that how we can choose the electrodes and fluxes for a particular weld by using ASME Section 2 Part C.

-
Regards
Ansari Intekhab Alam

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...