Saturday, December 24, 2011

Re: Re: [MW:13290] Surface roughness measurement instruments.


Hi

For measuring surface profile gauge go for

1. Elcometer model 223 Surface profile gauge digital (after blasting)

2. Elcometer DFT model no. 456 for Dry film thickness (after priming /
painting)

3. Elcometer model 319 RH calculator.Dew point to measure dew point ,
surface temp, ambient temp and relative humidity

4. Elcometer model 138 Bresle Set for checking salt contamination.



On Sat, 24 Dec 2011 10:00:35 +0530 wrote
>Dear Mr. Rao,
>
>There are portable surface roughness measuring instruments to measure as
required.
>
>UK based Rank Taylor Hobson instruments are available in India.
>
>SrinivasanSent from BlackBerry® on AirtelFrom: Vasantharao

Sender: materials-welding@googlegroups.com
Date: Thu, 22 Dec 2011 15:38:40 +0530 (IST)To: materials-
welding@googlegroups.comReplyTo:
materials-welding@googlegroups.com
Subject: [MW:13256] Surface roughness measurement instruments.
>Dear Experts,
I work as inspection
Engineer. When i go for Blasting inspection, contractor provided me profile
comparator for surface roughness measurement.
Contractor do Grit blasting in the shop.
I need to measure surface roughness - 75-100 microns Painting system No#1
50-75 microns Painting system No#2

Queries

Q 1: Comparator is enough for surface roughness measurements.
Q2: Is any other tools available for roughness measurement?.
Q3: What is the normal industry practice.


Pl. provide your valuable suggestions as i'm new for painting
activities.

Rao.






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951
Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...