Re: [MW:13376] Hydro test for different pressure

Mr. kanagarajan
please insure the following points
1. The piping class i.e. pipe thickness and rating
2. second check the piping matergaly if the one cs and other high
alloy such as ss etc then in ss some specicaly requiremetn such as DM
water etc

regards,
satyendra

On 12/28/11, Kanagarajan G <g.kanagarajan@gmail.com> wrote:
>>
>> Hi,
>>
>> Shall we carryout two different hydro pressure packs together in one hydro
>> test for the maximum one.
>>
>> For example, One test pack 30 PSI and another test pack 200 PSI.(Material
>> same)
>>
>> Regards,
>>
>> Kanagarajan.G
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...