Friday, December 30, 2011

Re: [MW:13366] Room Temp/High temp Properties & allowable stresses in P92 pipes

Check in ASME section II-A and II-D
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: Ved Bhushan Arora [vbarora48@gmail.com]
  Sent: 30/12/2011 09:52 ZE5B
  To: materials-welding@googlegroups.com
  Subject: [MW:13365] Room Temp/High temp Properties & allowable stresses in P92 pipes


Dear All
 
I need the P92 pipe material properties , physical , mechanical, high temp & allowable stresses etc.
 
Thanks
 
Ved Bhushan Arora

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...