Check the Pipe system rating(pipe class).If both are same technically you can go ahead with hydrotesting together.But still you need to get the designers approval.

On Wed, Dec 28, 2011 at 11:08 AM, Kanagarajan G <g.kanagarajan@gmail.com> wrote:
Hi,
 
Shall we carryout two different hydro pressure packs together in one hydro test for the maximum one.
 
For example, One test pack 30 PSI and another test pack 200 PSI.(Material same)
 
Regards,
 
Kanagarajan.G


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...