Inconels are high nickel. The colour you are observing should be the colour of Ni.

Srinivasan
Sent from BlackBerry® on Airtel

-----Original Message-----
From: Usman Anwar <mualhrpk@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Sun, 25 Dec 2011 04:49:26
To: Materials & Welding<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:13303] about innconel X750HT GASKET

Dear All,
Please conform me what is the natural color of X750HT.ASME 16.20 Table
19 tell us that its have no color. but we received gasket of this
material which looks like silver but data sheet says its not silver.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...