Sunday, December 25, 2011

Re: [MW:13300] Back purge for CuproNickel welding

Yes it is required back purging,you can use Nitrogen for purging.

On Sat, Dec 24, 2011 at 9:09 PM, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:
Hi friends
 
I am establishing a welding procedure for welding of 90-10 Cu-Ni 6mm thick tubes, UNS C70600 as per ASME SecIX.
All joints are single sided joints and i will be welding them with TIG: ER CuNi filler wire.
 
My only query was that do i need to back purge the weld joints ?
 
Regards
 
Prem S Nautiyal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...