[MW:13373] Failure Of Root bend test of Welding (CS to SS)

Dear Sir,
 
Advance happy new year to all.
 
I have done a PQR(As per ASME Sec ix) of 6", Sa106 GrB to Sa 312 TP 316L. One of the root bend of the same failed.
 
Consumable used: ErNiCr-3. 
 
Tesile strength T1=507 and T2=514MPa(Min Rqd 415MPa);
 
Hardness:
Sa106 Gr B side p.metal: 160,151,147
Sa106 Gr B side HAZ:160,156,156
Weld: 193,170,165
Sa312 TP316L P.metal: 175, 175,181
Sa312 TP316L HAZ: 165,151,151
Face bends are satisfactory.
 
One root bend satisfactory.
 
Please give me the possible reasons and the precautions on further doing the PQR.
 
Regards,
 
Hareesh K V

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...