Tuesday, December 27, 2011

[MW:13329] Ductility dip crack

Dear Experts,
Please shortly discuss about ductility dip crack. I know it is relatet to Ni-base alloys and austenitic stainless steels.
Does anyone know another name for this kind of crack?
 
Regrds

--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66282127
Fax: +98-21-66282779
 
Please don't print this e-mail unless you really need to. BeGreen!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]