I found the ollowing lines in an welding article on orbital
welding, that for a cryogenic fluid carrier, inner pipes
were chosen of 4306 stainless steel, diameters between 84
to 273 mm.L = 11,5 m / 6 m).Thickness (mm) 2.9 .Inner pipes
were supposed to be in contact with cryogenic fluid. With
different cryogenic temperatures: 1.8 to 80 K .xxxx
Conlcuding remark was "Practioner should pay attention about
Chemical composition to avoid "Marangoni effect" during welding.

Plz. educate me, what is Marangoni Effec and its relation with
weld material composition.?

Regards.
ANIL BARIK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...