Re: [MW:12638] Procedure for welding of sailhard material..........

Dear Mr.Kalyan..
 
Sailhard is the mateiral used for liner plates..hence most of the time only fillet weld or plug weld only.. Generally E 7018(SMAW)/ER 70S-2(GMAW) is used for this welding.
 
BR,
MSMS
 
 
 


 
On Fri, Oct 7, 2011 at 2:30 PM, kalyan vvv <vvvkalli@gmail.com> wrote:
Dear experts,
Could any one solve my doubts.........
     1)What are the welding consumables to be used for SAILHARD material?
     2)what is the procedure to weld SAILHARD plate material more than 10
         mm thick?               

--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
HYDERABAD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...