Sunday, October 2, 2011

Re: [MW:12603] Tension Test Requirement for SA 283 Gr.C plates



Dear Sir,

Two Tension test one in Traverse and another Longitudinal rolling direction  is enough



Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951


From: asad azmi <azmiasadayub@gmail.com>
Sent: Sun, 02 Oct 2011 11:28:28
To: materials-welding@googlegroups.com
Subject: Re: [MW:12601] Tension Test Requirement for SA 283 Gr.C plates
is the para 15.1.3 of SA 6 is applicable here.
 
 
please advice.
 
Regards
 
 
On Wed, Sep 28, 2011 at 7:39 PM, Pieper QSI <pieper-qsi@kpnmail.nl> wrote:

It seems to me that when every plate has similar heat and plate number they will be produced from a coil, especially when the thickness is 6 mm.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens asad azmi
Verzonden: woensdag 28 september 2011 16:29
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12573] Tension Test Requirement for SA 283 Gr.C plates

 

SA 20 is not applicable here.



 

On Wed, Sep 28, 2011 at 2:10 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

One tension test coupon shall be taken from each plate-as-rolled (para 11.1.1 of SA20).

 

Note: plate-as-rolled— the quantity of plate product rolled at one time, either from an individual slab or directly from an ingot.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, September 28, 2011 3:59 PM
To: materials-welding@googlegroups.com
Subject: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates

 

Dear All,

 

Greetings.

 

 

As per MTC for the plates material - SA283GR C,  for a single Heat number( 10K22884)  total 15 Nos of plates are supplied having plate no. 15942 

 

Description of Goods- Hot rolled steel plates with sheared edges. Plates are in Non Heatreated  condition.

 

MTC is showing only  2 tension test results.

 

Please clarify whether only two tension test are acceptable OR there shall be 15 nos of tension test for 15 plates.( 1 tension test for each plate)

 

Thanks & Regards

 

Asad Azmi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...