Monday, March 28, 2011

RE: [MW:10508] Lethal Service / ASME Sec VIII Div 1

No(refer note under UW2), it shall be the responsibility of the user and/or his designated agent to determine if it is lethal. If determined as lethal, the user and/or his designated agent [see U-2(a)] shall so advise the designer and/or Manufacturer. It shall be the responsibility of the Manufacturer to comply with the applicable Code provisions.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vino Varghese
Sent: Monday, March 28, 2011 11:10 AM
To: materials-welding@googlegroups.com
Subject: [MW:10507] Lethal Service / ASME Sec VIII Div 1

 

Dear All,

 

We are maufacturing a U-Stamp Pressure Vessel in accordance to ASME Sec VIII, Div 1.

Service: Sour Service

 

Query: How can you differentiate between an Sour Service with Lethal Service?

All Lethal Service requires PWHT and 100% RT for butt welds for Pressure Parts.

 

Do all Sour Service are Lethal in Nature?

 

Regards

Vino - Doha

 

 