Re: Re: [MW:5457] storage condition of E6013

Rutile does not require any holding temperature
It is not a Low Hydrogen type electrode
If you do require a low hydrogen deposit then you should change your consumable to a basic type electrode
Best Regards

PHIL CHEW

Global Segment Manager -Transport ,Shipbuilding,M&R

ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB

Tel: +44 (0) 7584 219132

email: PHIL.CHEW@esab.net

ESAB Holdings Ltd is a company registered in England and Wales . Co registration no 1687590 Registered Office: 322 High Holborn, London , UK , WC1V 7PB www.esab.comPlease consider the environment before printing this email.


  From: mahendran p [pmahe_79@yahoo.co.in]
  Sent: 08/06/2010 10:06 ZE5B
  To: materials-welding@googlegroups.com
  Subject: Re: Re: [MW:5437] storage condition of E6013


Dear Mr.Phil,
                   Does it require any holding temperature? I ever read in one std/code but not sure.
 
Thanks.
 
P.Mahendran.

--- On Mon, 7/6/10, Phil.Chew@esab.net <Phil.Chew@esab.net> wrote:

From: Phil.Chew@esab.net <Phil.Chew@esab.net>
Subject: Re: Re: [MW:5421] storage condition of E6013
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Monday, 7 June, 2010, 12:30 PM

I am an ESAB employee and I can confirm that you should not bake a E6013 stick electrode
This is a rutile type electrode and does not require baking
Best Regards

PHIL CHEW

Global Segment Manager -Transport ,Shipbuilding,M&R

ESAB Holdings Ltd, 322 High Holborn, London, UK, WC1V 7PB

Tel: +44 (0) 7584 219132

email: PHIL.CHEW@esab.net

ESAB Holdings Ltd is a company registered in England and Wales . Co registration no 1687590 Registered Office: 322 High Holborn, London , UK , WC1V 7PB www.esab.comPlease consider the environment before printing this email.

  From: sugu puma [pumamy@yahoo.com]
  Sent: 06/06/2010 07:21 MST
  To: materials-welding@googlegroups.com
  Subject: Re: Re: [MW:5416] storage condition of E6013


are they sure you said cannot baking in oven..............?,what the manufacture recommendation said?

From: john rodrigues <johnrodrigues2@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, June 6, 2010 3:39:15 PM
Subject: Re: Re: [MW:5412] storage condition of E6013

Hello,
E6013 is rutile type electrode and it does not require baking.
Regards.
joh

On Sun, 06 Jun 2010 09:09:34 +0530 wrote
>Dear all,
The baking temperature is 350 - holding temperature 150,see the manufacture rules and regulations before open the box of electrode cartoon,this is all low hydrogen electrode using,followup according manufacture recommendation and also take look in AWS D1.1.

From,
M.Sugumar


From: Sandeep Kp
To: materials-welding@googlegroups.com
Sent: Sat, June 5, 2010 10:34:30 PM
Subject: [MW:5401] storage condition of E6013


Dear all,
Let me know the baking & holding temperature of E6013 electrodes of ESAB.


Regds,

Sandeep.k.p







--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.









--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.

ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it.

ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...