On Thu, Jun 17, 2010 at 3:31 PM, Bhatti BM (Bashir) at Aera <BMBhatti@aeraenergy.com> wrote:
--
Tht depends on which specifiction/code you are following.
Folks,
We doing Mockup procedure before actual welding, what type tests are required to qualify the welding procedure
I was looking for welding procedures for and filler metals
CS A-106-B and 2 ¼ Cr ,
CS A-106-B and 410
CS A-106-B and 13 Cr
CS A-106-B and 9CR
Thanks , Bashbhat
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/