Thursday, June 17, 2010

Re: [MW:5631] Equipment Design Life

You have to know the corrosion rate and other degardation factors in order to estimate the design life.
The NBIC code is giving some instructions abou the calculation of the remaining life of pressure equipment which could help
Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for "Phirke, Praphulla D (GE Oil & Gas)" <praphulla.phirke@ge.com>"Phirke, Praphulla D (GE Oil & Gas)" <praphulla.phirke@ge.com>


          "Phirke, Praphulla D (GE Oil & Gas)" <praphulla.phirke@ge.com>
          Sent by: materials-welding@googlegroups.com

          17/06/2010 07:28

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

[MW:5627] Equipment Design Life

Ref


Dear Team members
Can anyone guide me how to calculate the equipment design life?
In one of the project , Customer has mentioned in the specifications about the design life as per attached file.

Please guide me how to design a equipment according to this requirements.

Thanks
Praphulla

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
(See attached file: Design Life.pdf)

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...