Wednesday, June 16, 2010

Re: [MW:5611] Tube to tube sheet welding

Hi,
 
As per ASME Sec IX QW 193 MLP dimension required by the design, it does not provide the dimension of MLP.  Generaly accepted minimum leak path is 70% of tube thickness.

Regards.
Abraham John

On Tue, Jun 15, 2010 at 9:18 PM, Shadab Alam Ansari (Welding Engineer) <shadabansarialam@gmail.com> wrote:
In Tube to tube sheet weld joint what is the minimum leak path
distance as per ASME SEC-IX.

Regards
Shadab Alam Ansari
Welding Engineer
Olayan Descon

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...