Hi
Kindly see the following-
If impact testing is not required, both non essential & supplementary variables shall be mentioned on WPS but for any change requalification is not required,
If impact testing is required, for any change in supplementary variables, requalification of WPS is required.
Should you have furhter quarries, pls ask me.
Regards
Manpreet Singh
On Mon, 14 Jun 2010 08:46:44 +0530 wrote
>Dear All
in QW 250-QW280 in ASME sec IX,SOME VARIABLES ARE NON ESSENTIAL & SUPPLEMENTARY IN SAME TIME.e.g in current
WHICH ONE SHALL BE CONSIDERED?HOW INTERPRETED?
REGARD ADVANCES
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Kindly see the following-
If impact testing is not required, both non essential & supplementary variables shall be mentioned on WPS but for any change requalification is not required,
If impact testing is required, for any change in supplementary variables, requalification of WPS is required.
Should you have furhter quarries, pls ask me.
Regards
Manpreet Singh
On Mon, 14 Jun 2010 08:46:44 +0530 wrote
>Dear All
in QW 250-QW280 in ASME sec IX,SOME VARIABLES ARE NON ESSENTIAL & SUPPLEMENTARY IN SAME TIME.e.g in current
WHICH ONE SHALL BE CONSIDERED?HOW INTERPRETED?
REGARD ADVANCES
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments