Sunday, June 13, 2010

Re: [MW:5573] swsi IQI wire

it is OK, becourse you can se a thinner IQI wire ( image quality indicater) the requried.

Regards, jimmy


On 13 June 2010 15:59, krishna <wiqw@rediffmail.com> wrote:
HI frnds,
Here we have a job of wall thickness of 11mm (SWSI) we are using IQI 10 ISO 16.
so for 2 % sensitivity 11x2% =0.22
if we see the chart of wire type IQI there is no 0.22 wire dia but
while review of film we see 4th wire i.e 0.20 so is it acceptable or not.
thnx,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...