Re: [MW:5559] Buttering of weld joints

Mr. Das,
Buttering is a technique in which weld is applied to the surface in order to acheive desired properties or required dimensions.

For example in fit-up/butt joint, if distance between two butting members is excess, buttering is done on one member to reduce the gap.

Buttering is also done on surfaces to provide metallurgically compatible weld metal for subsequent completion of weld.

Regards.

John






On Sat, 12 Jun 2010 18:22:35 +0530 wrote
>



Dear Sir

Can anyone describe me what is "BUTTERING" stands
for in welding joint. If it is done before depositing the weld metal on job, is
it necessary to remove the same by back chipping.









--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

Unknown said...

Dear All

I have the following queries regarding Buttering:

1) Can we use buttering during pipe joint bevel preparation?
2) Whether there will be any chance of crack formation due to this?
3) Is there any code reference for the same?

Regards
Harikrishnan N S

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...