Re: [MW:5526] Charpy for A53

what is your code of construction and thickness involved? and also provide MDMT, not operating temperature.

On Thu, Jun 10, 2010 at 7:13 PM, Emilio Cerato <ecerato@hotmail.com> wrote:

Dear All
I need to do a WPS for piping, This pipe drives ammonia.
Is necesary to do impact test?
The material is ASTM A53 GrB
The temperature of operation is -30ºC
I use E7018-1 for weld.
Thanks
 
Emilio Cerato



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...