Re: [MW:5517] EN Material Grouping

Dear all,
EN the materials are grouped as per EN 15608 Welding - Guidelines for
a metallic materials grouping system.


Rgds
Sudhakar

Sent from my iPhone

On 10-Jun-2010, at 5:21 PM, "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com
> wrote:

> Refer EN 10027-part1 & 2 Designation systems for steel
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-
> welding@googlegroups.com] On Behalf Of limesh M
> Sent: Thursday, June 10, 2010 2:26 PM
> To: Materials & Welding
> Subject: [MW:5513] EN Material Grouping
>
> Dear All,
>
> From where I can get EN material group number details.
>
> Thanks and Regards
>
> Filtered by Hosted Filtering
>
>
> --
> To post to this group, send email to materials-
> welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel
> views and meant for educational purposes only, Users must take their
> own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...