Hello Mr. Bagesh,
 
Yes  Casting valves can be used, but it depends on the design pressure of your pipelines.
For high-pressure services , you need to have  high quality castings.
 
Also if you are using WCB casting with high strength pipe material like APl5L Gr. B X42. X52 & X65. you must take into account the reduce pressure rating of WCB material compared with pipe material.
Also ASME B16.34 has not considered  , I am not exactly sure , but I think about 3 mm as corrosion allowance for valve body thickness calculation.
For higher corrosion allowance you must inform the manufacturer.
 
On the forging issue, you have an advantage regards to quality of valve body compared with castings, but there is higher cost involved.
 
hope this helps
 

Kind regards

Rahul Pisat
Piping Specialist
Plant Design

Akzo Nobel Technology & Engineering B.V.
Postal address: PO Box 9300, 6800 SB  Arnhem, the Netherlands
Visiting address: Velperweg 76, 6824 BM Arnhem, the Netherlands

T +31 26 366 4706, F +31 26 366 3401,
Visit our website @ www.akzonobel.com/te  

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of AGUSTIN JIMENEZ
Sent: woensdag 9 juni 2010 19:24
To: materials-welding@googlegroups.com
Subject: Re: [MW:5500] Casting materials for Valves for ASME B31.4 and B31.8

Hi Bagesh.
I am agree with Jorge, in Venezuela we use ASTM A216 Gr. WCB or WCC for petroleum liquid and gas too, if there are corrosive ambient choose other material for example Stainless steel.
And A105 <2" diameter.
 
Agustin


De: Jorge Mejía Lema <jmejialema@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: mié, junio 9, 2010 11:41:04 AM
Asunto: Re: [MW:5496] Casting materials for Valves for ASME B31.4 and B31.8

I have been working for the Colombian ECOPETROL Pipe Line for 20 years, we use ASTM A216 Gr. WCB for valves from 2 to 24 inches diameter and ASTM A 105 less than 2 inches diameter. We transport Crude Oil, ACPM, Gasoline, GLP, Natural Gas, Nafta, Jet A1, Kerosene, Diesel.
Regards,
jml

2010/6/8 Bagesh <bagesh.kmr@gmail.com>

Dear All,

            Would like to discuss the selection of Valve casting materials for the Pipelines project meant for transportation of Liquids hydrocarbons and Gas,

The Pipe materials used are High strength steels of API 5L Gr. B X42,X52, X65 etc, depending on the requirement of licensor, How to get the correct casting materials for valves, The pressure and temp. Ratings are according to ASME B16.34.

===================
Bagesh Kumar

Seoul 135985

===================

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Jorge Mejia Lema.
Especialista IV Mecánico.
Gerencia Tanques.
PBX: +57 (1) 3215801 Ext. 4094
FAX: +57 (1) 3215913
Cell: 3174793091
Carrera 11 No.71-73 Piso 10
ITANSUCA PROYECTOS DE INGENIERIA Ltda.
Bogotá, Colombia, Sur América
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 
____________________________________________________________________________
This email has been scanned for Viruses and Spam. For more information
please contact your local Business Unit Information Security representative.
____________________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...