Hi,
 
Cannot possible to use the Same WPS.
 
May be you can write the Prequalified WPS for the 3G position ,
 
Or
 
You can qualify the WPS for the 3G position to qualify the welders
 
Or
 
You can go for the Production mock up
 
Regards,
 
Babu
Singapore
 
----- Original Message -----
Sent: Tuesday, June 08, 2010 12:48 PM
Subject: [MW:5437] Welder Qualification in 2G - 3G

Dear friend,
 
I have a query as below.
 
Our customer had establised a WPS/PQR  in 2G position - 16 mm thk plate.
 
They want qualification test for welders in 3G position (6mm Thk Plate), Can we allow the same?
 
Electrode: E7018
Coupen : IS 2062 Gr. B plate
Ref. Code : AWS D1.1
 
Regards,
Checks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...