Re: [MW:5476] welding A335 P91 with Carbon steel

Dear Mauricio
 
As per my Knowledge best Filelr wire to use : ER 90S-B9 for GTAW
 
E9015-B9 FOR SMAW.
 
RGDS
M.M.REDDY
QA/QC INSPECTOR (MECHANICAL)
METHANOL PLANT
DAMIATTA - EGYPT
0020168194532



 
On Mon, Jun 7, 2010 at 12:31 AM, mauricio padilla <mauricio_padilla_f@yahoo.com> wrote:
Sirs,
 
I have a question about welding dissimilar material:
 
One Metal:          A335 P91 ----------------------------------        PNumber 15E
Second Metal      MSS SP75 WPHY-70  ---------------        Snumber 1
 
Wall thickness                                                              36.53 mm
 
Which ones are the best  FILLER METAL for   GTAW?
 
Which ones are the best  FILLER METAL for   SMAW?
 
 
Is it necessary PWHT?
 
Please give a tips.
 
Best Regards
 
Mauricio

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...