Dear Kaushik,
 
As per AWS D 1.1  for procedure qualification the position is an essential variable.  Hence you should have WPS in 3G position to qualify the welder in 3G position.  As per ASME sec. IX position is not essential variable for WPS.
 
Regards
 
N.V. PRASAD

On Tue, Jun 8, 2010 at 7:48 AM, Kaushik Patel <checkspatel@gmail.com> wrote:
Dear friend,
 
I have a query as below.
 
Our customer had establised a WPS/PQR  in 2G position - 16 mm thk plate.
 
They want qualification test for welders in 3G position (6mm Thk Plate), Can we allow the same?
 
Electrode: E7018
Coupen : IS 2062 Gr. B plate
Ref. Code : AWS D1.1
 
Regards,
Checks

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...