Re: [MW:5457] Hardness requirement for P1 material

As per NACE MR0175 max hardness acceptable for any component is 22HRC

On Tue, Jun 8, 2010 at 9:47 AM, Sakib <sakib321@gmail.com> wrote:
is NACE MR 0175 has hardness of all materials ?
can somebody share this with me ?

--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...