RE: [MW:5437] Fillet Weld Minimum thickness requirement

Check the code mate

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram
(Mumbai - PIPING)
Sent: Tuesday, 8 June 2010 2:36 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:5436] Fillet Weld Minimum thickness requirement

What is your code of construction and type of attachment? If it is ASME Sec
VIII div 1, refer UW13 and UW16, if it is B31.3 refer para 328.5 and
associated figures

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Srinivas Engr
Sent: Monday, June 07, 2010 2:03 PM
To: Materials & Welding
Subject: [MW:5426] Fillet Weld Minimum thickness requirement

Dear All

What is the minimum fillet weld throat thickness requirement.?

For example Base material thickness is 10mm, for fillet weld, How much
throat thickness is required?
pl explain...

Thanks
Srinivas


Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...