Tuesday, June 8, 2010

RE: [MW:5436] Fillet Weld Minimum thickness requirement

What is your code of construction and type of attachment? If it is ASME Sec VIII div 1, refer UW13 and UW16, if it is B31.3 refer para 328.5 and associated figures

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Srinivas Engr
Sent: Monday, June 07, 2010 2:03 PM
To: Materials & Welding
Subject: [MW:5426] Fillet Weld Minimum thickness requirement

Dear All

What is the minimum fillet weld throat thickness requirement.?

For example Base material thickness is 10mm, for fillet weld, How much throat thickness is required?
pl explain...

Thanks
Srinivas


Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...